Water penetration behavior in water-assisted injection molding (WAIM) : A study of product quality for different process and material parameters / Sofie Sannen in INTERNATIONAL POLYMER PROCESSING, Vol. XXVII, N° 5 (11/2012)
[article]
Titre : Water penetration behavior in water-assisted injection molding (WAIM) : A study of product quality for different process and material parameters Type de document : texte imprimé Auteurs : Sofie Sannen, Auteur ; M. de Munck, Auteur ; Peter Van Puyvelde, Auteur ; J. de Keyzer, Auteur Année de publication : 2012 Article en page(s) : p. 602-616 Note générale : Bibliogr. Langues : Anglais (eng) Catégories : Matières plastiques -- Moulage par injection
Matières plastiques -- Moulage par injection assistée par eau
Moulage par injection -- Défauts
PolypropylèneTags : 'Moulage injection assisté eau' Polypropylène 'Comportement pénétration 'Epaisseur paroi résiduelle' 'Formation défaut pièce' 'Mesure pression 'Débit volume' Viscosité 'Fluidité cisaillement' Index. décimale : 668.4 Plastiques, vinyles Résumé : This study investigates the relation between water penetration behavior and product quality in water-assisted injection molding (WAIM) for different process and material parameters. The principle mechanisms responsible for both building up the residual wall thickness (RWT) and formation of part defects as well as the influence of these process and material parameters on the RWT and occurrence of part defects could be revealed. This is done by relating the measurements of water pressure and water volume flow rate, visualizing in-mold variations during water injection, to both the part weight and a visual inspection of part cross-sections, for different process settings and materials. It was found that the RWT as well as the formation of part defects depend on the polymer resistance, since the variation of the latter leads to a change in both the water bubble width and velocity. On the one hand, the resistance is determined by the process parameters having an influence on the amount of melt ahead of the water bubble, depending on injector opening time, water volume flow rate and water injection delay time. On the other hand, the resistance also depends on the friction between the polymer chains, which is determined by the zero-shear viscosity and the shear thinning behavior of the polymer. In addition, the occurrence of part defects is directly related to the polymer crystallization behavior. The resulting product quality therefore depends on a combination of the process parameters and the applied material. Note de contenu : - EXPERIMENTAL : Material ans set-up - Methodology
- RESULTS AND DISCUSSION : Injector opening time - Influence of material parametersDOI : 10.3139/217.2622 En ligne : https://drive.google.com/file/d/1QMi2LZqb5pZ-u5u4ggioD88OQUFJCeov/view?usp=drive [...] Format de la ressource électronique : Permalink : https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=16643
in INTERNATIONAL POLYMER PROCESSING > Vol. XXVII, N° 5 (11/2012) . - p. 602-616[article]Réservation
Réserver ce document
Exemplaires (1)
Code-barres Cote Support Localisation Section Disponibilité 14335 - Périodique Bibliothèque principale Documentaires Disponible