Titre : |
The effect of weathering and thermal treatment on the scratch recovery characteristics of clearcoats |
Type de document : |
texte imprimé |
Auteurs : |
Christopher M. Seubert, Auteur ; Mark E. Nichols, Auteur ; K. Henderson, Auteur ; Markus Mechtel, Auteur ; Thomas Klimmasch, Auteur ; Torsten Pohl, Auteur |
Année de publication : |
2010 |
Article en page(s) : |
p. 159-166 |
Note générale : |
Bibliogr. |
Langues : |
Américain (ame) |
Tags : |
'Peinture automobile' Clearcoat Uréthane 'Résistance éraflure' 'Nano-éraflure' 'Macro-éraflure' Guérison |
Index. décimale : |
667.9 Revêtements et enduits |
Résumé : |
The scratch and scratch recovery characteristics of two clearcoats, a polyurethane and an acrylic/melamine/silane clearcoat, were measured by a variety of methods. On most size scales tested, the polyurethane possessed superior scratch and mar resistance. The polyurethane also possessed improved scratch recovery after warming for 2 h at 60°C. After 2000 h of accelerated weathering, the scratch recovery characteristics of the polyurethane were largely maintained, while the acrylic/melamine/silane showed a significant drop in scratch recovery performance. Performance of both coatings was related to T g, hardness, and crosslink density. |
DOI : |
10.1007/s11998-009-9190-4 |
En ligne : |
https://link.springer.com/content/pdf/10.1007%2Fs11998-009-9190-4.pdf |
Format de la ressource électronique : |
Pdf |
Permalink : |
https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=9062 |
in JOURNAL OF COATINGS TECHNOLOGY AND RESEARCH > Vol. 7, N° 2 (03/2010) . - p. 159-166