The impact of acid rain on vegetable tanned leather / Yanping Gao in JOURNAL OF THE SOCIETY OF LEATHER TECHNOLOGISTS & CHEMISTS (JSLTC), Vol. 100, N° 3 (05-06/2016)
[article]
Titre : The impact of acid rain on vegetable tanned leather Type de document : texte imprimé Auteurs : Yanping Gao, Auteur ; Yang Shuang, Auteur ; Teng Bo, Auteur ; Jinwei Zhang, Auteur ; Jian Xiaoyun, Auteur ; Lucretia Miu, Auteur ; Carmen Gaidau, Auteur ; Wuyong Chen, Auteur Année de publication : 2016 Article en page(s) : p. 131-135 Note générale : Bibliogr. Langues : Anglais (eng) Catégories : Analyse thermique
Cuirs et peaux -- Analyse
Cuirs et peaux -- Détérioration
Cuirs et peaux -- Propriétés mécaniques
Essais accélérés (technologie)
Essais dynamiques
Morphologie (matériaux)
Pluies acides
Tannage végétalIndex. décimale : 675.2 Préparation du cuir naturel. Tannage Résumé : Artificial acid rain was chosen to simulate the influences of gaseous pollutants on vegetable-tanned leather. The vegetable-tanned leather samples were soaked in the artificial acid rain for 0, 5, 10, 15, 20 and 25 days, at 50°C and 100% relative humidity conditions. Then, these samples were evaluated by various analytical methods. Micro hot table (MHT), differential scanning calorimetry (DSC) and thermogravimetry (TG) were used to evaluate the influences of acid rain on thermal behaviours. Damage to mechanical properties were also analyzed by a standard method. Fourier transform infrared spectroscopy (FTIR) and optical microscopy were used to investigate the changes of structural and histological properties during ageing. With the extension of ageing time, thermal stability was gradually reduced to lower values, including shrinkage temperature, thermal denaturing temperature, associated enthalpy and temperature of maximum decomposition rate. ln addition, mechanical properties such as tensile strength, tear strength and elongation at break also gradually decreased. The FTIR results showed that, during the ageing process, the amide 1 and amide 11 bands of collagen were gradually shifted to lower numbers, indicating increasingly serious damage to the structure of the peptide chain corresponding to obvious fibril breakages which were also detected through optical microscopy. Note de contenu : - EXPERIMENTAL METHODOLOGY : Materials - Sampling - Preparation of artificial acid rain - Leather ageing process - Analytical methodology
- RESULTS AND DISCUSSION : Thermal analysis - Mechanical properties - Morphology and structureEn ligne : https://drive.google.com/file/d/1qSZYzF-OT_TZl-1LmxTyAgXz_8UA3qET/view?usp=drive [...] Format de la ressource électronique : Permalink : https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=26446
in JOURNAL OF THE SOCIETY OF LEATHER TECHNOLOGISTS & CHEMISTS (JSLTC) > Vol. 100, N° 3 (05-06/2016) . - p. 131-135[article]Réservation