Synthesis and urea-loading of a novel biosuperabsorbent polymer based on leather waste / Hu Zaiyin in JOURNAL OF THE SOCIETY OF LEATHER TECHNOLOGISTS & CHEMISTS (JSLTC), Vol. 99, N° 2 (03-04/2015)
[article]
Titre : Synthesis and urea-loading of a novel biosuperabsorbent polymer based on leather waste Type de document : texte imprimé Auteurs : Hu Zaiyin, Auteur ; Yi Shouhong, Auteur ; Hu Wei, Auteur ; Yuling Tang, Auteur ; Wang Ru, Auteur Année de publication : 2015 Article en page(s) : p. 51-57 Note générale : Bibliogr. Langues : Anglais (eng) Catégories : Absorbants et adsorbants
Copolymère acide acrylique acrylamide
Copolymères -- Synthèse
Cuirs et peaux -- Déchets -- Recyclage
Greffage (chimie)
Humidité -- Absorption:Eau -- Absorption
UréeIndex. décimale : 675 Technologie du cuir et de la fourrure Résumé : In order to develop an eco-friendly polymer, a novel superabsorbent polymer was synthesized by grafting the alkaline hydrolysis product of Leather waste (LW) to a copolymer of acrylic acid (AA) and acrylamide (Afv1)(PLW-g-(AA-co-AM) with microwave method assistance. The morphology of the samples was examined by scanning electron microscopy (SEM). Through a single factor experiment, various factors were explored which may affect the water absorption of such a superabsorbent polymer du ring preparation. The results showed that the optimum technological conditions of synthesizing PLW-g-(AA-co-AM) were : dosage of LW 15wt.% of total monomer mass, cross-linking agent 0.06wt.°/0 of monomer mass, neutralization degree 75%, AA: AM= 6 :1, initiator 0.6wt.% of monomer mass. According to this procedure, the PLW-g-(AA-co-AM) with a water-absorbency of 1191.5g/g and salt-absorbency of 94.4g/g was obtained. The product was used as adsorbant for urea, the urea load rate reached 87.76% when the concentration of urea was 10g/L. Meanwhile, the release of urea from the loaded PLW-g-(AA-co-AM) in deionized water exhibited specific release properties. Note de contenu : - EXPERIMENTAL PROCEDURE : Materials - Swelling measurements : Tea-bag method - Instrumental analysis
- RESULTS AND DISCUSSIONS : Optimization of the grafting conditions - Loading and release of ureaEn ligne : https://drive.google.com/file/d/1PiVWaSmKFsQTY_zL8lgdvGzkXTi9x7V3/view?usp=drive [...] Format de la ressource électronique : Permalink : https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=23741
in JOURNAL OF THE SOCIETY OF LEATHER TECHNOLOGISTS & CHEMISTS (JSLTC) > Vol. 99, N° 2 (03-04/2015) . - p. 51-57[article]Réservation
Réserver ce document
Exemplaires (1)
Code-barres Cote Support Localisation Section Disponibilité 17138 - Périodique Bibliothèque principale Documentaires Disponible