Thermal and tensile behavior of HD-PE films containing iron (III) acetylacetonate after UV irradiation / D. Kiryakova in INTERNATIONAL POLYMER PROCESSING, Vol. XXIX, N° 5 (11/2014)
[article]
Titre : Thermal and tensile behavior of HD-PE films containing iron (III) acetylacetonate after UV irradiation Type de document : texte imprimé Auteurs : D. Kiryakova, Auteur ; S. Mihaleva, Auteur ; A. Atanassov, Auteur ; M. Tavlieva, Auteur Année de publication : 2014 Article en page(s) : p. 588-593 Note générale : Bibliogr. Langues : Anglais (eng) Catégories : Acétylacétone
Chlorure de fer
Photo-oxydation
Polyéthylène haute densité
Polymères -- Propriétés mécaniques
Polymères -- Propriétés thermiques
Traction (mécanique)Index. décimale : 668.9 Polymères Résumé : The thermal, tensile and other properties of high density polyethylene films containing iron (III) acetylacetonate as pro-oxidant additive have been studied after exposure to UV irradiation for up to 300?h. The effect of photooxidation on polyethylene films with and without pro-oxidant was estimated by Fourier transform infrared spectroscopy, X-ray diffraction analysis, Differential scanning calorimeter measurements and the tensile properties. It was observed that UV irradiation had almost no effect on the melting temperature of the different samples. After exposure, the degree of crystallinity increased from 69% to 72% for the initial polyethylene samples without pro-oxidant additive and by 3% for the samples containing iron (III) acetylacetonate. It was found that the increase in the carbonyl index of initial HDPE was not significant even after 60?h exposure to UV irradiation while samples with pro-oxidant suffered substantial degradation still for 35?h. It was observed that the decrease of the tensile strength is more pronounced for the samples with pro-oxidant under irradiation for 60 to 70?h. The films containing pro-oxidant lose ?90% of its initial elongation at break after 35?h exposure. Note de contenu : - Materials
- Sample preparation
- UV exposition
- Differential Scanning Calorimeter (DSC) Measurements
- Fourier Transform Infrared Spectroscopy (FT-IR)
- X-Ray Structure Analysis
- Tensile Properties
- Melt Index
- Sol-Gel AnalysisDOI : 10.3139/217.2900 En ligne : https://drive.google.com/file/d/1bxWp7Be3YyGJfJZqFj8pJIxjlGPaE43F/view?usp=drive [...] Format de la ressource électronique : Permalink : https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=22224
in INTERNATIONAL POLYMER PROCESSING > Vol. XXIX, N° 5 (11/2014) . - p. 588-593[article]Réservation