Accueil
Détail de l'auteur
Auteur C. R. Tomachuk |
Documents disponibles écrits par cet auteur
Ajouter le résultat dans votre panier Affiner la recherche
Morphology and corrosion resistance of Cr(III)-based conversion treatments for electrogalvanized steel / C. R. Tomachuk in JOURNAL OF COATINGS TECHNOLOGY AND RESEARCH, Vol. 7, N° 4 (07/2010)
[article]
Titre : Morphology and corrosion resistance of Cr(III)-based conversion treatments for electrogalvanized steel Type de document : texte imprimé Auteurs : C. R. Tomachuk, Auteur ; C. I. Elsner, Auteur ; A. R. di Sarli, Auteur ; O. B. Ferraz, Auteur Année de publication : 2010 Article en page(s) : p. 493-502 Note générale : Bibliogr. Langues : Américain (ame) Catégories : Acier L'acier est un alliage métallique utilisé dans les domaines de la construction métallique et de la construction mécanique.
L'acier est constitué d'au moins deux éléments, le fer, très majoritaire, et le carbone, dans des proportions comprises entre 0,02 % et 2 % en masse1.
C'est essentiellement la teneur en carbone qui confère à l'alliage les propriétés du métal qu'on appelle "acier". Il existe d’autres métaux à base de fer qui ne sont pas des aciers comme les fontes et les ferronickels par exemple.
Chimie écologique
Chrome trivalent
Corrosion
Dépôt électrolytique
Revêtements:Peinture
Spectroscopie d'impédance électrochimique
Zinc
ZingageTags : 'Traitement de conversion' Corrosion 'Chrome III' 'Technologies vertes' 'Spectroscopie d'impédance 'Embrun salin' NaCl Zinc 'Acier électrogalvnisé' Index. décimale : 667.9 Revêtements et enduits Résumé : The effectiveness of Cr(VI)-based passivation treatments is well accepted but there are many problems with regard to their environmental suitability. Because these compounds are carcinogenic and toxic, eco-friendly systems capable of replacing them are being evaluated. In this work, the corrosion behavior in 0.5 M NaCl solution of zinc coatings deposited from a free-cyanide alkaline bath and treated with Cr3+ based passivation coatings were characterized through DC and EIS techniques. The salt spray test as well as studies of the surface structure and chemical composition were also performed. From these analyses it was inferred that (1) the green-colored Cr3+ passivated coatings provide better corrosion resistance than the yellow- and blue-colored coatings, and (2) together with an adequate painting system, they could be a less polluting and less toxic alternative to traditional chromate coatings. DOI : 10.1007/s11998-009-9213-1 En ligne : https://link.springer.com/content/pdf/10.1007%2Fs11998-009-9213-1.pdf Format de la ressource électronique : Permalink : https://e-campus.itech.fr/pmb/opac_css/index.php?lvl=notice_display&id=9772
in JOURNAL OF COATINGS TECHNOLOGY AND RESEARCH > Vol. 7, N° 4 (07/2010) . - p. 493-502[article]Réservation
Réserver ce document
Exemplaires (1)
Code-barres Cote Support Localisation Section Disponibilité 012362 - Périodique Bibliothèque principale Documentaires Disponible